16 COMMON WELDING DEFECTS AND HOW TO FIX THEM

Like many stages in metal fabrication, welding must be performed accurately and consistently to ensure the final product performs effectively in service. Conversely, even minor welding defects can render welding fabrication parts unusable or, worse, cause serious damage to large structures and construction projects.

Welding defects mainly arise from both internal and external factors, including human skills, equipment, materials, procedures, and environmental conditions. Once the root causes are correctly identified, effective corrective solutions can be applied.

  1. Cracks 

Cracks

Causes:

  • Metal shrinkage during cooling
  • Impurities or hydrogen in the weld metal
  • Poor joint design
  • Excessively rapid cooling

 

Solutions:

  • Control cooling rate (preheating/post-heating)
  • Use appropriate, low-impurity filler materials
  • Design joints to reduce residual stress
  • Reweld following standard procedures

 

  1. Underfill

Underfill welding

Causes:

  • Low welding current
  • Excessive welding speed
  • Insufficient filler material
  • Excessively wide weld groove

 

Solutions:

  • Increase current to ensure full melting
  • Reduce travel speed to allow proper fill
  • Select suitable electrode/wire diameter
  • Apply multi-pass welding for deep grooves

 

  1. Undercut

Undercut

Causes:

  • Excessive current
  • High travel speed
  • Improper electrode angle
  • Excessive arc length

 

Solutions:

  • Reduce current and travel speed
  • Maintain electrode angle at 5–15°
  • Apply weaving technique
  • Avoid excessively long arc length

 

  1. Burn-Through

Burn-through

Causes:

  • Excessive current
  • Thin base material
  • Slow welding speed
  • Improper welding technique

 

Solutions:

  • Reduce current or use pulsed mode
  • Increase electrode travel speed
  • Use backing bars or backing strips
  • Select TIG or MIG welding for thin materials

 

  1. Overlaps

Overlaps in welding

Causes:

  • Oversized electrode
  • Incorrect electrode angle
  • Excessively slow travel speed
  • Poor welding technique

 

Solutions:

  • Use a smaller electrode
  • Adjust electrode angle
  • Increase welding speed to prevent metal overflow

 

  1. Porosity

porosity

Causes:

  • Insufficient shielding gas
  • Contaminated surfaces (oil, rust, moisture)
  • Unstable arc

 

Solutions:

  • Clean surfaces thoroughly before welding
  • Control shielding gas flow rate
  • Maintain stable electrode position and proper angle

 

  1. Arc Strikes

Arc strike

Causes:

  • Arc initiation outside the weld zone
  • Improper arc starting location

Solutions:

  • Initiate the arc at the correct location
  • Remove arc strikes by grinding after welding

 

  1. Excessive Spatter

excessive spatter

Causes:

  • Excessive arc length
  • High current
  • Unstable shielding gas

 

Solutions:

  • Keep electrode close to the workpiece
  • Adjust current appropriately
  • Inspect and stabilize the shielding gas system

 

  1. Lack of Penetration

Lack of penetration

Causes:

  • Low welding current
  • Excessive travel speed
  • Improper groove design

 

Solutions:

  • Increase welding current
  • Reduce travel speed
  • Modify groove design as required

 

  1. Slag Inclusion

Slag Inclusions

Causes:

  • Inadequate cleaning between passes
  • Incorrect electrode angle
  • Insufficient arc energy

 

Solutions:

  • Clean thoroughly between weld passes
  • Adjust electrode angle
  • Ensure proper arc control

 

  1. Mis-alignment

Mis-alignment

Causes:

  • Incorrect positioning
  • Inadequate clamping or fixturing

 

Solutions:

  • Verify fixture alignment before welding
  • Use secure clamps or jigs

 

  1. Lack of Fusion

lack of fusion

Causes:

  • Low welding current
  • High travel speed
  • Improper joint geometry

 

Solutions:

  • Increase current
  • Reduce travel speed
  • Adjust joint configuration

 

  1. Undersized Weld

under size in welding

Causes:

  • Insufficient filler material
  • Incorrect groove design

 

Solutions:

  • Increase filler metal deposition
  • Review and correct groove design

 

  1. Start/Stop Defects

 

start and stop welding defects

Causes:

  • Inconsistent hand movement
  • Sudden arc termination

 

Solutions:

  • Improve operator control
  • Apply proper weld termination techniques

 

  1. Heat Tint (Stainless Steel)

Heat tints

Cause:

Thickening of the natural oxide layer on stainless steel due to welding heat

Solutions:

  • Clean using specialized chemical agents
  • Perform post-weld stainless steel passivation

 

  1. Rust on weld (Stainless Steel)

Rust on weld

Causes:

  • No surface treatment after welding
  • Exposure to corrosive environments

 

Solutions:

  • Acid pickling
  • Stainless steel passivation
  • Surface protection using organic, polymer, or inorganic coatings, such as epoxy coatings, clear lacquers, or specialized anti-rust sprays

The above are common welding defects encountered during welding fabrication parts production. Whether you are a welder, mechanical engineer, QC/QA specialist, contractor, or manufacturing business owner, understanding these defects is essential to selecting appropriate fabrication methods and corrective measures to ensure high-quality, safe, and reliable production outcomes.

If you need high-quality welding parts manufacturer offering tailored metal solutions that meet international standards.

Contact Newinds:

  • Email: sales@newindscorp.com
  • Phone/Whatsapp/Zalo: Ann Yen +84 344 644 077
LinkedIn
Facebook
Twitter